Rock wool consists of 60% diabase, 20% limestone and 20% coke. After being melted in a high-temperature furnace at 1500~2000℃, it is sprayed into filaments with a diameter of 0.005 mm, and then pressed the filaments into a plate with a density of 80~ 1000 kg/m³.High-pressure water jet cutting is the [Read More]